1. SiC Heating rod is heated in the air after the formation of a silicon oxide film compact surface,Into a protective film to protect the antioxidant, play a role in prolonging life. In recent years, our company developed a variety of silicon carbide coating to prevent cracking, for a variety of gas furnace.
2. Continuous use of silicon carbide, hoping to slow increasing resistance to maintain long life.
3. Globar as far as possible in parallel. If the silicon carbide with different resistance and series resistance of silicon carbide rod load, resulting in a rapid increase in a silicon carbide rod resistance, shorter life expectancy.
4. After the silicon carbide rod with the temperature higher lifetime is shorter, so in the furnace temperature super 1400 DEG C, accelerate the oxidation rate, shorten life. Use note try not to let the silicon carbide surface temperature is too high.